3N4 along with decomposition of SiNxOy occurred, resulting in a considerable decrease in weight and a catastrophic decrease in strength for the oxidized fibers."/>
Science and Technology on Advanced Ceramic Fibers and Composites Laboratory,National University of Defense Technology,Science and Technology on Advanced Ceramic Fibers and Composites Laboratory,National University of Defense Technology,Science and Technology on Advanced Ceramic Fibers and Composites Laboratory,National University of Defense Technology
[Hu Xuan, Shao Changwei, Wang Jun. Effects of oxidative behavior on the strength and thermal resistance of continuous silicon nitride fibers[J]. Rare Metal Materials and Engineering,2018,47(S2):232~237.]