2 and Al2O3 with a three-dimensional network structure, and TiC-coated Fe are filled in the three-dimensional ZTA ceramics skeleton. The inefficacy mechanism of ZTA-TiC-Fe: the phase transformation of Fe and ZrO2 occurs at about 750℃; The volume changing of phase transformation of Fe and ZrO2 during heating and cooling and the internal stress release caused by the different thermal expansion coefficients of each component lead to the thermal expansion of the ZTA-TiC-Fe cermet. In the aerobic environment, the oxidation rate of Fe phase in the surface layer increases when the temperature exceeds 550℃, resulting in porous red-brown Fe2O3. The oxidation of Fe phase produces about 8 times volume expansion, resulting in the irreversible rupture of three-dimensional ceramic skeleton."/>
1.Key Laboratory of Cryogenic Engineering, Institute of Physical and Chemical Technology, Chinese Academy of Sciences;2.Key Laboratory of Cryogenic Engineering, Institute of Physical and Chemical Technology, Chinese Academy of Sciences, Beijing 100190
[Guannan, Li Jiangtao. High Temperature Stability of ZTA-TiC-Fe Cermets Synthesized by High Gravity Combustion[J]. Rare Metal Materials and Engineering,2020,49(2):582~588.]
DOI:10.12442/j. issn.1002-185X. QH20190035