2Nd and Al11Nd3phases in the matrix and the grain refinement in Mg-Al-Ca alloy, and the amounts of Al2Nd and Al11Nd3 phases increase with the increase of Nd addition. The average grain size of alloys changed from 4.80 μm without Nd to 2.39 μm when added 1.76% Nd. The mechanical properties at room temperature were improved due to the precipitation of second phases and grain refinement. With increment of Nd, the tensile strength increased from 267 MPa to 304 MPa, the yield strength increased from 144 MPa to 203 MPa and the elongation decreased from 20.0 % to 16.9% at room temperature in these alloys. At 150℃, the tensile strength increased from 192 MPa to 229 MPa, the yield strength increased from 140 MPa to 159 MPa and the elongation decreased from 48.6 % to 29.3% with increasing Nd content."/>
1.School of Materials Science and Engineering,Beijing Institute of Technology;2.College of Materials Science and Engineering,Chongqing University
[Donghu Yang, Xianhua Chen, Xiaoyang Xu, Chaoyue Zhao. Effect of Nd on microstructure and mechanical properties of Mg-Al-Ca alloy[J]. Rare Metal Materials and Engineering,2020,49(1):1~9.]
DOI:10.12442/j. issn.1002-185X.20180734