17Al12 phase. Moreover, the content of beta phase increases with the increase of Al content. As a result, the corrosion resistance of the three alloys was enhanced with the increase of the β phase. The Mg-15%Al alloy has the best corrosion resistance, and Mg-9%Al is the worst. The oxide film formed on the all as cast Mg-Al alloys surface after hydrogen evolution testing for 72 h in 3.5 wt.% NaCl. Furthermore, the stability of the film increased with the increase of Al content."/>
College of Materials Science and Engineering,Taiyuan University of Science and Technology,Taiyuan,Shanxi,College of Materials Science and Engineering,Taiyuan University of Science and Technology,Taiyuan,Shanxi,College of Materials Science and Engineering,Taiyuan University of Science and Technology,Taiyuan,Shanxi,College of Materials Science and Engineering,Taiyuan University of Science and Technology,Taiyuan,Shanxi,College of Materials Science and Engineering,Taiyuan University of Science and Technology,Taiyuan,Shanxi,College of Materials Science and Engineering,Taiyuan University of Science and Technology,Taiyuan,Shanxi,College of Materials Science and Engineering,Taiyuan University of Science and Technology,Taiyuan,Shanxi
TG146.22
[Guo Yanping, Wang Yaning, Wang Quanle, Wang lin, Dong Zhaobo, Fang Daqing, Liu Baosheng. Investigation on the microstructure and corrosion behavior of the as-cast Mg-xAl(x=9, 12, 15) alloys[J]. Rare Metal Materials and Engineering,2018,47(8):2531~2536.]
DOI:[doi]