41Sm5 phase is found because of Sm addition, Sm promotes the precipitation of Mg5Gd. After solution-aging treatment, the coarsening eutectic structures at grain boundary were dissolved and the precipitation dispersed homogeneous. The finer grain size is observed when content of Sm come to 3wt%. Some of Mg5Gd phase become short rod-like when Sm addition is 5wt%. Under the same experimental temperature, the strength of tested alloys increases at fist and then decrease, and peak strength present when content of Sm is 3wt%. For the same alloy, with increasing of test temperature, the strength increase at fist and then decrease too. When Sm content is 0~1wt%, the temperature of tensile strength peak is 200℃ and the temperature is 250℃ when Sm content is 3~5wt%. There are abnormal temperature effects in tensile tests, the effect is reinforced and the temperature of tensile strength peak rise with the Sm addition."/>
School of Materials Science and Engineering,Henan University of Science and Technology
[Zhu Li-min, Li Quan-an, Zhou Yao, Yan Jing-long. Effect of Sm on microstructures and mechanical properties of Mg-10Gd-0.5Zr alloy[J]. Rare Metal Materials and Engineering,2019,48(1):171~176.]
DOI:10.12442/j. issn.1002-185X.20170425