f=498mA ,the welding speed V=1200mm/min and the electron beam is Ib=6.8mA, the welding joint without the addition of scanning can obtain good forming and no macro porosity defects.Under the same conditions compared to other add scan mode of welding, derived welding in the process of adding triangle wave scanning, we can not only obtain the forming good macro porosity defects in the welded joints, and the welding joint of the hardness values and tensile strength is improved. The average tensile strength of welded joint is 323.55MPa, and the fracture strength of the joint is 71.5%, The extension rate is up to 86.8% of the elongation of base metal.which is the weakest part of the weld zone."/>
National Defence Key Disciplines Laboratory of Light Alloy Processing Science and Technology,Nanchang Hangkong University,Nanchang,National Defence Key Disciplines Laboratory of Light Alloy Processing Science and Technology,Nanchang Hangkong University,Nanchang,National Defence Key Disciplines Laboratory of Light Alloy Processing Science and Technology,Nanchang Hangkong University,Nanchang,National Defence Key Disciplines Laboratory of Light Alloy Processing Science and Technology,Nanchang Hangkong University,Nanchang
[ZHANG Ziyang, WANG Shanlin, KE Liming, Li juan. Effect of scanning mode on Microstructure and mechanical properties of 2198 Al-Li alloy joint fabricated by electron beam welding[J]. Rare Metal Materials and Engineering,2018,47(7):2245~2251.]
DOI:[doi]