x could be detected on the surface. It finally arrived that after a storage time of nearly 12 years, the main part of the tritide film were striped by inner evolved helium bubbles."/>
School of National Defence Science and Technology,Southwest University of Science and Technology,School of National Defence Science and Technology,Southwest University of Science and Technology,School of National Defence Science and Technology,Southwest University of Science and Technology,School of National Defence Science and Technology,Southwest University of Science and Technology,Institute of Chemical Mateirals, China Academy of Engineering Physics,
[Liu Yang, Yang Tao, Wang Xuan, Wu Fengjuan, Liu Jiwei, Wang Boyu. Influence of the storage time of tritium titanium target on its damage characteristics in a D-T neutron generator[J]. Rare Metal Materials and Engineering,2017,46(6):1731~1733.]