4Sr phase; 2) The morphology of the Al4Sr phase on Al-10Sr master alloy changed from acicular shape to small blocks with the addition of RE to 4.0wt %; 3) The grain size of primary silicon on Al-20Si alloy was refined into a range of 13.81-37.61μm, and the average grain size was 24.58μm with a homogeneous distribution during modification by using the Al-10Sr-4RE master alloy; 4) It was found that after adding RE, the Al4Sr phase distribution became more homogeneous, and it exhibited better modification effect on Al-20Si alloy."/>
[Qiu Zhihua, Li Yunlong, Chen Huan, Chen Jianchun, Zhang Guodong, Pan Chunxu. Effect of RE on microstructures of Al-10Sr master alloy and the application in Al-20Si alloy casting[J]. Rare Metal Materials and Engineering,2017,46(5):1310~1314.]