2). The mixed oxides mainly exist in the form of amorphous phase. The average crystallite size reaches a minimum value at the nominal La content of 30 mol%, while the oxide coating shows the highest electrochemical activity."/>
[Long Ping, Xu Likun, Li Qingfen, Xue Lili, Song Hongqing. Effect of Microstructure on Electrochemical Activity of Ru-La Oxide Coatings on Ti Substrate[J]. Rare Metal Materials and Engineering,2013,42(6):1185~1189.]
DOI:[doi]