g=129 kJ/mol,速率常數(shù)K=1.28×10-8 m4·s-1?;诒∧げ牧系木ЯIL模型和能量各向異性特性,解釋了(001)取向晶粒得以快速生長的原因,且發(fā)現(xiàn)這些快速生長的晶粒與S晶粒呈40°<111>取向關系。;Based on electron backscattered diffraction (EBSD) and grain growth model of thin film materials, grain sizes and growth thermo-kinetics were investigated during annealing with different heating rates in high-voltage anode aluminum foil. Results show that the grain growth exponent n=4, activation energy Qg=129 kJ/mol and rate constant K=1.28×10-8 m4·s-1 are calculated by the typical isothermal grain growth equation. Based on grain growth model of thin film materials and energy anisotropy, the reasons for the rapid growth of (001) oriented grains are well explained, and a typical 40°<111> misorientation relationship with S-grains is found."/>