Effect of Cu/Al Thickness-ratio on Deformation Behavior and Bonding Properties of Corrugated Roll Bonding Cu/Al Clad Plates
Author:
Affiliation:

1.College of Mechanical Engineering,Taiyuan University of Science and Technology;2.College of Mechanical and Vehicle Engineering,Taiyuan University of Technology

Fund Project:

  • 摘要
  • |
  • 圖/表
  • |
  • 訪問統(tǒng)計
  • |
  • 參考文獻(xiàn)
  • |
  • 相似文獻(xiàn)
  • |
  • 引證文獻(xiàn)
  • |
  • 資源附件
  • |
  • 文章評論
    摘要:

    本文通過剪切強(qiáng)度測試、剪切斷面顯微觀察和有限元仿真等手段對不同Cu/Al層厚比下波紋輥軋制(CRB)Cu/Al復(fù)合板的金屬的變形行為和界面結(jié)合性能進(jìn)行了研究。結(jié)果發(fā)現(xiàn),CRB過程中界面處形成了局部強(qiáng)正應(yīng)力和多個“搓軋區(qū)”,促進(jìn)了復(fù)合板的塑性變形和界面結(jié)合。增大Cu/Al層厚比可提升Cu層的變形率和波谷界面處的正應(yīng)力,有利于降低Cu/Al復(fù)合板的翹曲程度,并增強(qiáng)界面的整體結(jié)合性能。當(dāng)層厚比從2:10增加到2:4時,界面剪切強(qiáng)度從40.39 MPa上升到47.24 MPa,但界面剪切強(qiáng)度的波動逐漸增大。

    Abstract:

    The deformation behavior and interfacial bonding properties of Cu/Al clad plates with different Cu/Al thickness-ratio by corrugated roll bonding (CRB) were investigated by shear strength test, microstructure observation of shear section and finite element simulation. The results show that increasing the Cu/Al thickness-ratio is beneficial to reduce the warpage of the Cu/Al clad plates and improve the overall bonding properties of the interface. When the Cu/Al thickness-ratio is 2:4, the Cu/Al clad plate hardly warps, and the shear strength reaches 47.24 MPa. As the Cu/Al thickness-ratio decreases, the rolling deformation zone expands and the rolling force is dispersed. Thus, the peak value of normal stress and average shear strength at the interface both decrease gradually. The shear stress generated by multiple "cross-shear" zones and the local strong normal stress formed at the interfaces during the CRB process significantly promote the plastic deformation and interface bonding of the clad plates.

    參考文獻(xiàn)
    相似文獻(xiàn)
    引證文獻(xiàn)
引用本文

高翔宇,黃志權(quán),江連運(yùn),王濤,馬立峰. Cu/Al層厚比對波紋輥軋制Cu/Al復(fù)合板變形行為和結(jié)合性能的影響[J].稀有金屬材料與工程,2023,52(4):1447~1454.[Gao Xiangyu, Huang Zhiquan, Jiang Lianyun, Wang Tao, Ma Lifeng. Effect of Cu/Al Thickness-ratio on Deformation Behavior and Bonding Properties of Corrugated Roll Bonding Cu/Al Clad Plates[J]. Rare Metal Materials and Engineering,2023,52(4):1447~1454.]
DOI:10.12442/j. issn.1002-185X.20220319

復(fù)制
文章指標(biāo)
  • 點(diǎn)擊次數(shù):
  • 下載次數(shù):
  • HTML閱讀次數(shù):
  • 引用次數(shù):
歷史
  • 收稿日期:2022-04-16
  • 最后修改日期:2022-07-19
  • 錄用日期:2022-08-11
  • 在線發(fā)布日期: 2023-05-01
  • 出版日期: 2023-04-25