Influence of Heat Treatment Temperature on Bonding and Oxidation Resistance of Diamond Coated TiO2 Film
Author:
Affiliation:

Hunan University,Hunan University,Hunan University,Hunan University,Hunan University

Fund Project:

  • 摘要
  • |
  • 圖/表
  • |
  • 訪問統(tǒng)計
  • |
  • 參考文獻
  • |
  • 相似文獻
  • |
  • 引證文獻
  • |
  • 資源附件
  • |
  • 文章評論
    摘要:

    利用溶膠-凝膠法在金剛石表面涂覆一層TiO2薄膜,通過掃描電鏡、紅外光譜、拉曼光譜、X-射線衍射、光電子能譜、綜合熱分析、破裂強度試驗等測試方法,表征了熱處理溫度對金剛石表面TiO2薄膜的形貌、相組成、相變、與基體金剛石的成鍵和涂膜后金剛石抗氧化性能的影響。研究結(jié)果表明:熱處理溫度上升到600℃時,金剛石表面的TiO2薄膜會由無定型態(tài)轉(zhuǎn)變?yōu)橹旅艿匿J鈦礦相薄膜,TiO2與金剛石基體形成Ti-O-C化學鍵合;熱處理溫度為800℃時,TiO2薄膜依然為銳鈦礦相,金剛石基體產(chǎn)生石墨化,石墨C也能與TiO2薄膜形成Ti-O-C化學鍵合,但薄膜開始出現(xiàn)裂紋。同時,TiO2薄膜的熱處理溫度對金剛石在空氣中的抗氧化性能有較大影響,當熱處理溫度在600℃時,金剛石的起始氧化溫度達到最大值754℃,在空氣中800℃氧化0.5h金剛石的氧化失重率達到最小值6.7wt.%,抗壓強度達到最大值15.7N。

    Abstract:

    TiO2 films were prepared on the surface of diamond through sol-gel method. The effect of heat treatment temperature on morphology, phase composition, phase transition, bonding with diamond, and oxidation resistance of diamond coated with TiO2 films of TiO2 film of diamond surface were characterized through SEM, FTIR , Raman spectroscopy, X-ray diffraction analysis, XPS, TG-DSC, fracturing strength. The results showed that when the heat treatment temperature rose to 600℃, TiO2 film of diamond surface would change from amorphous state to a dense anatase films and Ti-O-C chemical bond was formed between TiO2 and diamond substrate. When the heat treatment temperature rose to 800℃, TiO2 film was still anatase phase, graphitization of diamond substrate generared, graphitization C could form Ti-O-C chemical bond with TiO2 film, however, TiO2 film began to emerge cracks. Meanwhile, the heat treatment temperature of TiO2 films had a greater impact on the oxidation resistance of diamond in the air. When the heat treatment temperature was at 600℃, diamond initial oxidation temperature reached a maximum 754 ℃.After diamond coated with TiO2 films oxidized at 800℃ for 0.5h in the air, the weight loss rate and compressive strength was 6.7wt.% and 15.7N, respectively.

    參考文獻
    相似文獻
    引證文獻
引用本文

劉小磐,宋冬冬,萬隆,龐先兵,李爭.熱處理溫度對表面涂覆TiO2薄膜的金剛石成鍵及抗氧化性能影響[J].稀有金屬材料與工程,2017,46(1):195~200.[liuxiaopan, songdongdong, wanlong, pangxianbing, lizheng. Influence of Heat Treatment Temperature on Bonding and Oxidation Resistance of Diamond Coated TiO2 Film[J]. Rare Metal Materials and Engineering,2017,46(1):195~200.]
DOI:[doi]

復制
文章指標
  • 點擊次數(shù):
  • 下載次數(shù):
  • HTML閱讀次數(shù):
  • 引用次數(shù):
歷史
  • 收稿日期:2014-10-13
  • 最后修改日期:2014-11-17
  • 錄用日期:2014-12-25
  • 在線發(fā)布日期: 2017-03-16
  • 出版日期: