The effects of the mold temperature and the forming speed on semi-solid 6061 alloy forging were studied by means of software DEFORM-3D. The results show that when the temperature of semi-solid slurry is kept at 650 oC, the mold temperature 400 oC, and the forming speed 50 mm/s, an excellent part can be obtained. The HV hardness value of semi-solid forging parts with T5 treatment is 2166 MPa, 170.5% higher than that of the normal low-press cast parts. The simulation results are well in agreement with the experiment.
參考文獻
相似文獻
引證文獻
引用本文
劉 靜,王 平.6061鋁合金半固態(tài)模鍛成形的DEFORM-3D模擬與驗證[J].稀有金屬材料與工程,2014,43(10):2455~2458.[Liu Jing, Wang Ping. DEFORM-3D Simulation of Forging of Semi-solid 6061 Alloy and Validation[J]. Rare Metal Materials and Engineering,2014,43(10):2455~2458.] DOI:[doi]