最新色国产精品精品视频,中文字幕日韩一区二区不卡,亚洲有码转帖,夜夜躁日日躁狠狠久久av,中国凸偷窥xxxx自由视频

+高級(jí)檢索
基于JMatPro軟件不同B含量下Co-8.8Al-9.8W合金析出相的熱力學(xué)模擬計(jì)算
DOI:
作者:
作者單位:

蘭州理工大學(xué),蘭州理工大學(xué)

作者簡介:

通訊作者:

中圖分類號(hào):

TG146.1 6

基金項(xiàng)目:


Thermodynamic Simulation Calculation of Co-8.8Al-9.8W alloy with different B content based on JMatPro software
Author:
Affiliation:

Lanzhou University of Technology,Lanzhou University of Technology

Fund Project:

  • 摘要
  • |
  • 圖/表
  • |
  • 訪問統(tǒng)計(jì)
  • |
  • 參考文獻(xiàn)
  • |
  • 相似文獻(xiàn)
  • |
  • 引證文獻(xiàn)
  • |
  • 資源附件
  • |
  • 文章評論
    摘要:

    為研究B元素對新型鈷基高溫合金析出相的影響,本文基于JMatPro熱力學(xué)模擬計(jì)算軟件對不同B含量下Co-8.8Al-9.8W合金的平衡相析出行為進(jìn)行了研究。結(jié)果表明:B含量的增加,會(huì)導(dǎo)致γ相、μ-Co7W6相析出溫度的降低,并減少γ相、μ-Co7W6相析出量,相反會(huì)提高η-Co3Al相的析出溫度及析出量。針對這一計(jì)算結(jié)果,本文作者從B對平衡相中各元素的影響,硼化物等角度分析,給出了解釋。分析認(rèn)為隨著B含量的增加,使γ相析出時(shí)固液平衡相中各元素的含量相差越來越多,要滿足γ相的形核和長大只有降低溫度增加過冷度來實(shí)現(xiàn)。從而導(dǎo)致隨著B含量的增加,γ相的含量越來越少,析出溫度越來越低。硼化物的析出,固溶了大量的Co、W,使固液平衡相中Al的含量增加,促進(jìn)了Co3Al的析出。

    Abstract:

    In order to research the effect of boron additions on precipitation phases of New Co base superalloy. to save cost and to short period. The precipitation phases of Co-8.8Al-9.8W alloy with different B content have been studied by Thermodynamic Simulation Calculation of JMatPro software. The result shows that the precipitation temperature and precipitation quantity of γ phase and μ-Co7W6 phase becomes lower while the content of B increases. whereas the precipitation temperature and precipitation quantity of η-Co3Al phase becomes higher. Finally, the result has been explained from the factors of boride phases and the effect of B on composition of precipitation. Interpretation indicates that with the increase of B content,content of each element of Solid-liquid equilibrium phase has a growing difference when γ phase precipitates ,lowering the temperature increases, increasing the degree of super cooling, can make phase γ nucleation and growth. Thus with the increase of B content, the content of γ phase gets less and the precipitation temperature gets lower. The precipitation of borides leads a lot Co, W solid solution, which made a growth of Al in the solid-liquid equilibrium phase and promotes the precipitation of Co3Al.

    參考文獻(xiàn)
    相似文獻(xiàn)
    引證文獻(xiàn)
引用本文

徐仰濤,沙岐振.基于JMatPro軟件不同B含量下Co-8.8Al-9.8W合金析出相的熱力學(xué)模擬計(jì)算[J].稀有金屬材料與工程,2016,45(9):2332~2336.[xuyangtao, shaqizhen. Thermodynamic Simulation Calculation of Co-8.8Al-9.8W alloy with different B content based on JMatPro software[J]. Rare Metal Materials and Engineering,2016,45(9):2332~2336.]
DOI:[doi]

復(fù)制
文章指標(biāo)
  • 點(diǎn)擊次數(shù):
  • 下載次數(shù):
  • HTML閱讀次數(shù):
  • 引用次數(shù):
歷史
  • 收稿日期:2014-07-23
  • 最后修改日期:2014-08-18
  • 錄用日期:2014-09-28
  • 在線發(fā)布日期: 2016-10-09
  • 出版日期: