Ti45Al8Nb0.5B0.2C合金的組織及高溫氧化行為研究
DOI:
作者:
作者單位:

作者簡介:

通訊作者:

中圖分類號:

基金項目:

北京市教委高層次人才培養(yǎng)項目 (00900054R8002)


Microstructure and High Temperature Oxidation Behaviour of Ti45Al8Nb0.5B0.2C Alloy
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 圖/表
  • |
  • 訪問統(tǒng)計
  • |
  • 參考文獻(xiàn)
  • |
  • 相似文獻(xiàn)
  • |
  • 引證文獻(xiàn)
  • |
  • 資源附件
  • |
  • 文章評論
    摘要:

    研究了Ti45Al8Nb0.8B0.2C合金的組織及高溫氧化行為。XRD、SEM、TEM及EDS分析表明, 合金熱等靜壓后的組織為γ和α2相組成的片層組織, 片層團(tuán)晶粒內(nèi)部與層片團(tuán)晶界處存在條狀或點狀白色相TiB2; 高溫淬火合金發(fā)生α→γm相變, 在α+γ兩相區(qū)時效合金組織由不同取向的細(xì)小層片和層片交界處的α2相組成。氧化增重實驗及XRD、SEM分析表明, 合金在900和1000 ℃氧化100 h, 氧化反應(yīng)常數(shù)分別為0.001 92和0.316 37, 冪指數(shù)分別為1.1381和2.0076。合金在900 ℃氧化100 h后氧化層厚度大約為4 μm, 從外到內(nèi)依次為: 不連續(xù)的Al2O3層/Al2O3+TiO2混合層/富Nb層/基體。合金在1000 ℃氧化100 h后氧化層厚度大約為5 μm,從外到內(nèi)依次為:TiO2/Al2O3+TiO2/氮化物層/基體。

    Abstract:

    Microstructure and high temperature oxidation behaviour of Ti45Al8Nb0.5B0.2C alloy was investigated in this work. XRD, SEM, TEM and EDS analysis demonstrate that as-cast Ti46Al8Nb0.5B0.2C alloy after HIP has fully lamellar microstructure consisting of γ and α2 with point-like or ribbon-like TiB2 distributing in the colony or at grain boundary. When the alloy was treated at 1400 ℃ for 1 h and oil cooled from the single α filed leads to α→γm transformation and γm was aged in the α+γ two-phase field, alpha plates precipitated on all {111} planes of the γm to form fine microstructures. In addition to determination of the oxidation knetics by mass gain measurements, surface and cross-sectional morphologies of oxidizing layer formed was observed by SEM and the present phases in the scales were analyzed by XRD. Results show that oxidation reaction constant and power index for Ti46Al8Nb0.5B0.2C alloy oxidized at 900 ℃for 100 h were 0.00192 and 1.1381, respectively. However, oxidation reaction constant and power index for Ti46Al8Nb0.5B0.2C alloy oxidized at1000 ℃ for 100 h were 0.31637 and 2.0076, respectively. Oxidizing layer of Ti46Al8Nb0.5B0.2C alloy after 900℃, 100 h oxidation was about 4 μm and composed of four layer. The first layer is discontinous Al2O3, the second layer is the mixture of Al2O3 and TiO2, and the last is rich in Nb. Oxidizing layer of Ti46Al8Nb0.5B0.2C alloy after 1000 ℃, 100 h oxidation was about 5 μm and composed of 4 layer. The first layer is TiO2, the second layer is the mixture of Al2O3 and TiO2, and the third layer is nitride layer in sequence.

    參考文獻(xiàn)
    相似文獻(xiàn)
    引證文獻(xiàn)
引用本文

蘇香林,陳子勇,相志磊,聶祚仁. Ti45Al8Nb0.5B0.2C合金的組織及高溫氧化行為研究[J].稀有金屬材料與工程,2013,42(6):1178~1184.[Su Xianglin, Chen Ziyong, Xiang Zhilei, Nie Zuoren. Microstructure and High Temperature Oxidation Behaviour of Ti45Al8Nb0.5B0.2C Alloy[J]. Rare Metal Materials and Engineering,2013,42(6):1178~1184.]