The effects of sintering temperature,holding time and hot pressure on the density and mechanical properties of a hot pressed(PM)powder metallurgy 30vol%TiC\-p/W composite have been investigated. An optimum process for the preparation of 30vol%TiC\-p/W composite with higher strength and toughness has been devised.The 30vol%TiC\-p/W composite has excellent high temperature strength.This is attributed to a brittle ductile transision of the tungsten matrix combined with the strengthening effect of hard TiC particles in the W matrix.
參考文獻
相似文獻
引證文獻
引用本文
宋桂明 周玉. TiCp/W復合材料的制備工藝與力學性能[J].稀有金屬材料與工程,1999,(3):171~175.[Song Guiming, Zhou Yu, Wang Yujin, Lei Tingquan. Processing and Mechanical Properties of 30vol%TiC\-p/W Composite[J]. Rare Metal Materials and Engineering,1999,(3):171~175.] DOI:[doi]